Characterization

Inventory Classification
  • Materials Characterization
  • Surface analysis
  • Characterization

Contact surface profiler capable of measuring step height, roughness, waviness and other surface characteristics. Has a vertical measurement range from under 100 Å to 300 µm. Has a scan length of 8.1” and a scan speed of 1 to 25 µm/s. Also has a programmable force range of 1 to 50 mg.

University Tag Number: 
170492
Availability: 
Contact Custodian for availability
  • Greg Strommen
Location
Research II
Room Number: 
122C
Inventory Classification
  • Materials Characterization
  • Surface analysis
  • Characterization

The P-6 stylus profiler and surface analysis system offers a combination of advanced features for process development and manufacturing control of scientific research, photovoltaic solar manufacturing, data storage, MEMS, opto-electronics, and other industrial metrology applications.

University Tag Number: 
182973
Availability: 
Contact Custodian for availability
  • Seth Rasmussen
Location
Dunbar Hall
Room Number: 
58
Inventory Classification
  • Materials Characterization
  • Surface analysis
  • Characterization

The rolling thin film oven is used to measure the effect of heat and air on a moving film of semi-solid asphaltic material. The results of this treatment are determined from measurements of the asphalt properties before and after the test.

University Tag Number: 
172396
Availability: 
Contact Custodian for availability
  • Magdy Abdelrahman
Location
Civil & Industrial Engineering
Room Number: 
109